Who is this for?
Everyone. It is a "know" page, with one safe thing to do yourself: the magnet test.
Most car panels are steel. More and more bonnets, doors, guards and tailgates are aluminium, especially on newer and premium vehicles and some utes and trucks. The structure behind the panels often uses stronger steels that behave very differently when stressed or heated.
| Material | Where you find it | Behaviour in a dent | Heat | Repair implication |
|---|---|---|---|---|
| Mild steel | Older and many current outer panels | Stretches, usually forgiving, springs back in a predictable way | Tolerates controlled heat | Many small dents repairable without repaint |
| High-strength steel (HSS) | Doors, pillars, rails, some skins | Springs back more, harder to work | Heat limits set by the manufacturer | Specialist; follow the manufacturer's repair information |
| Ultra-high-strength and boron steel (UHSS) | Pillars, door intrusion beams, roof rails, safety cell | Very hard; can crack if forced; may be not repairable | Many manufacturers ban heat on it | Replace, do not straighten, in many cases; never a DIY job |
| Aluminium | Bonnets, doors, tailgates, guards, some whole bodies | Springs back less predictably, work-hardens, can crack; creases may mean replacement | Needs controlled low temperatures; no colour change to warn you | Specialist; many shops refuse or replace |
| Magnesium | Some internal parts (dash and seat frames, steering wheel cores) | Brittle | Burns; do not heat or grind | Not a panel DIY material |
| Carbon fibre and composites | Performance, premium and some EV panels, roofs, bonnets | Cracks and delaminates instead of denting; damage may be hidden | Heat can damage the resin | Often replace; repair is specialist |
| Galvanised steel | Many panels have a zinc coating for rust protection | Behaves like steel, but the zinc layer matters | Zinc burns off with heat and welding gives off fumes | Protection must be restored after repair |
Do this one thing yourself: the magnet test
Hold a fridge magnet or small magnet against the panel (put a thin cloth between so it cannot scratch). If it sticks firmly, it is steel. If it does not, it may be aluminium, a composite, or plastic filler or plastic. A bonnet that feels light is a clue too. A magnet cannot tell mild steel from high-strength steel, and it cannot tell you if there is filler hidden under the paint.
Other clues
- Owner's manual or the manufacturer's website often says which panels are aluminium.
- A dealer or repairer can look up the vehicle's build and repair information.
- Visible weave under the clear coat means carbon fibre; a thin, shiny, tapping sound can mean plastic or composite.
- Very thick, dented-in filler under a magnet can sound dull or feel different when tapped.
What this means for a dent
- Steel: small, shallow dents in good paint may be repairable without repainting by a trained technician.
- Aluminium: do not experiment. Cheap kits and heat tricks can crack the metal or the paint, and that is harder to put right afterwards. Some manufacturers say creases and kinks in some aluminium alloys mean replacing the panel.
- HSS, UHSS and boron steel: leave to the repairer. Many manufacturers restrict or ban straightening and heat on these steels and say to replace at factory seams.
- Any panel: creases, sharp edges and stretched metal are not DIY.
Pros and cons
| Good | Not so good |
|---|---|
|
|
Do and don't
| Do | Don't |
|---|---|
|
|
- The magnet does not stick (aluminium, plastic or composite)
- The damage is on a pillar, door beam, roof rail or other part of the safety structure
- There is a crease, kink or stretched metal
- You see cracked paint, exposed metal or rust
Coming next
- Panel-by-panel guide for popular models, and why some makers specify replacing instead of repairing.
Sources and further reading
- I-CAR: Working with boron-alloyed steel (UHSS)
- I-CAR: Straightening and heat, General Motors
- I-CAR: Straightening and heat, Volkswagen (aluminium limits)
- Vehicle maker repair information: Body Structure Materials and Allowed Operations
- Tomorrow's Technician: fixing dents in aluminium
- FenderBender: repair vs replace, carbon fibre
- Supplier guide: steel panel replacement process (zinc-rich weld-through coating)
Source links are for background only. Several are industry or supplier pages, so treat product claims with care. Technician sign-off: pending.